Materials & Grades

Spheroidal Graphite/Ductile Iron: Material Specification

Mechanical properties as measured on separately cast test bars

Material designation
EN 1563(Symbol)
India
IS 210
1978
Germany
DIN 1693
1973
UK
BS 2789
1985
USA
ASTM A536
1993
International
ISO 1083
1987
Tensile Strength
(N/mm2)
Elongation(%) Hardness(BHN)
EN-GJS 350-22 SG 350/22 350-22 350-22 350 22 < 150
EN-GJS 350-22LT SG 350/22 L GGG 35.3 350-22L40 350-22L 350 22 < 150
EN-GJS 400-18 SG 400/18 400-18 60-40-18 400-18 400 18 130-180
EN-GJS 400-18LT SG 400/18L GGG 40.3 100-18L20 400-18L 400 18 130-180
EN-GJS 400-15 SG 420/15 GGG 40 420-12 65-45-12 400-15 400 15 130-180
EN-GJS 450-10 SG 450/10 450-10 70-50-05 450-10 450 10 160-210
EN-GJS 500-7 SG 500/7 GGG 50 500-7 80-55-06 500-7 500 7 170-230
EN-GJS 600-3 SG 600/3 GGG 60 600-3 100-70-03 600-3 600 3 190-270
EN-GJS 700-2 SG 700/2 GGG 70 700-2 700-2 700 2 225-305
EN-GJS 800-2 SG 800/2 GGG 80 800-2 120-90-02 800-2 800 2 245-335
EN-GJS 900-2 SG 900/2 900-2 900-2 900 2 280-360

Cast Iron/ Grey Iron - Material Specification

Mechanical properties as measuresd on separately cast test bars

Material designation
EN 1561
India
IS 210
1993
Germany
DIN 1691
1973
UK
BS 1452
1990
USA
ASTM A48
1994
International
ISO 1085
1987
Tensile Strength(min)
(N/mm2)
Hardness(BHN)
EN-GLJ-150 FG 150 GG 15 Grade 150 25B 150 150 130 - 180
EN-GLJ-200 FG 200 GG 20 Grade 200 30B 200 200 160 - 220
EN-GLJ-250 FG 250 GG 25 Grade 250 35B 250 250 180 - 230
EN-GLJ-300 FG 300 GG 30 Grade 300 45B 300 300 180 - 230
EN-GLJ 350 FG 350 GG 35 Grade 350 50B 350 350 207 - 240